Helios is a 1 µm device. These are typical emissivity values to set on the instrument.
| Material / process | Typical temp (°C) | Emissivity ε |
|---|---|---|
| Molten glass in melting furnace | 1,400–1,600 | 0.95–0.97 |
| Glass bath, deep melt in forehearth and working end | 1,200–1,500 | 0.95–0.97 |
| Glass gobs leaving the feeder | 1,000–1,200 | 0.80–0.90 |
| Glass during forming, IS machine | 700–1,100 | 0.85–0.92 |
| Hot bottle just after moulding | 500–700 | 0.80–0.90 |
| Bottle at annealing lehr entrance | 500–600 | 0.85–0.92 |
| Furnace refractories: silica, AZS, alumina | 800–1,600 | 0.95–1.00 |
| Furnace crown refractories | 1,000–1,500 | 0.95–1.00 |
| Cast-iron moulds, oxidised | 500–700 | 0.70–0.90 |
| Material / process | Typical temp (°C) | Emissivity ε |
|---|---|---|
| Steel, oxidised scale | 800–1,200 | 0.60–0.90 |
| Steel, polished sheet | 500–900 | 0.30–0.40 |
| Stainless steel, bright | 500–900 | 0.30–0.40 |
| Steel, molten, clean surface | 1,500–1,650 | 0.30–0.40 |
| Iron, oxidised | 500–1,000 | 0.40–0.80 |
| Iron, unoxidised | 500–1,000 | 0.30–0.40 |
| Iron, molten | 1,300–1,550 | 0.30–0.40 |
| Cast iron, oxidised | 500–1,000 | 0.70–0.90 |
| Cast iron, unoxidised | 500–1,000 | 0.30–0.40 |
| Cast iron, molten | 1,300–1,500 | 0.30–0.40 |
| Aluminium, unoxidised or polished | 500–700 | 0.10–0.20 |
| Aluminium, oxidised | 500–700 | 0.25–0.45 |
| Aluminium, roughened | 500–700 | 0.20–0.80 |
| Copper, oxidised | 500–900 | 0.20–0.80 |
| Brass, oxidised | 500–800 | 0.55–0.65 |
| Nickel, oxidised | 600–1,100 | 0.80–0.90 |
| Nickel, electrolytic | 500–900 | 0.20–0.40 |
| Inconel, oxidised | 600–1,100 | 0.40–0.90 |
| Nickel superalloy Waspaloy, heated in air | 600–1,100 | 0.77–0.83 |
| Haynes alloy | 700–1,100 | 0.50–0.90 |
| Molybdenum, oxidised | 500–1,000 | 0.50–0.90 |
| Molybdenum, unoxidised | 800–1,500 | 0.25–0.35 |
| Titanium, polished | 500–900 | 0.50–0.75 |
| Tungsten, polished | 1,000–2,000 | 0.35–0.40 |
| Graphite | 500–1,500 | 0.80–0.90 |
| Material / process | Typical temp (°C) | Emissivity ε |
|---|---|---|
| Steam-reformer tubes, oxidised HP and HP-micro alloy | 900–1,000 | 0.85–0.86 |
| Cracker and heater tubes, oxidised HK40 and HP | 800–1,100 | 0.85–0.86 |